As specified in §§ 63.5710(d) and 63.5714(a), you must calculate point values using the formulas in the following table:
| For this operation—
| And this application method—
| Use this formula to calculate the MACT model plant value for each resin and gel coat—
|
|---|
| 1. Production resin, tooling resin | a. Atomized | 0.014 × (Resin HAP%)
2.425
|
| | b. Atomized, plus vacuum bagging with roll-out | 0.01185 × (Resin HAP%)
2.425
|
| | c. Atomized, plus vacuum bagging without roll-out | 0.00945 × (Resin HAP%)
2.425
|
| | d. Nonatomized | 0.014 × (Resin HAP%)
2.275
|
| | e. Nonatomized, plus vaccum bagging with roll-out | 0.0110 × (Resin HAP%)
2.275
|
| | f. Nonatomized, plus vacuum bagging without roll-out | 0.0076 × (Resin HAP%)
2.275
|
| 2. Pigmented gel coat, clear gel coat, tooling gel coat | All methods | 0.445 × (Gel coat HAP%)
1.675
|
[66 FR 44232, Aug. 22, 2001; 66 FR 50504, Oct. 3, 2001]