(a) The joint must be brought to brazing temperature in as short a time as possible to minimize oxidation.
(b) [Reserved]
[CGFR 68-82, 33 FR 18843, Dec. 18, 1968, as amended by USCG-2003-16630, 73 FR 65184, Oct. 31, 2008]
authority: 33 U.S.C. 1321(j), 1509;
43 U.S.C. 1333;
46 U.S.C. 3306,
3703; E.O. 12234, 45 FR 58801, 3 CFR, 1980 Comp., p. 277; E.O. 12777, 56 FR 54757, 3 CFR, 1991 Comp., p. 351; DHS Delegation No. 00170.1, Revision No. 01.4
source: CGFR 68-82, 33 FR 18843, Dec. 18, 1968, unless otherwise noted.
cite as: 46 CFR 56.75-15